ZrSe2 Crystal

SKU:
BLK-ZrSe2
Condition:
New
  • ZrSe2 crystals - Laarge size high purity ZrSe2 layered crystals - 2Dsemiconductors USA
  • ZrSe2 crystals - Laarge size high purity ZrSe2 layered crystals - 2Dsemiconductors USA
  • Raman spectrum of ZrSe2 crystals - Laarge size high purity ZrSe2 layered crystals - 2Dsemiconductors USA
  • XRD from ZrSe2 crystals - Laarge size high purity ZrSe2 layered crystals - 2Dsemiconductors USA
$590.00
Frequently bought together:

Description

ZrSe2 belongs to group-IV TMDCs family and adopts a stable 2H-hexagonal structure. ZrSe2 is 0.95 eV indirect gap semiconductor in the bulk form. These ZrSe2 crystals were designed and optimized at our facilities starting 2013 to achieve perfect electronic grade materials with: 1) excellent stoichiometry, 2) large single domain size, 3) single phase materials without any mixed phases or amorphous content, 4) unmatched purity -electronic grade (6N), 99.9999% confirmed purity. Our crystals exhibit sharpest Raman and XRD peaks in the commercial market proving the high quality of our materials.

Properties of ZrSe2 layered crystals

Sample size ~1cm combined
Material properties IR semiconductor (0.95 eV bulk)
Crystal structure 2H Hexagonal
Degree of exfoliation Easy exfoliation characteristics
Production method Modified flux zone growth (highest grade)
Other characteristics
  • Easy to exfoliate
  • High purity
  • Electronic and optical grade

 

Growth method matters> Flux zone or CVT growth method? Contamination of halides and point defects in layered crystals are well known cause for their reduced electronic mobility, reduced anisotropic response, poor e-h recombination, low-PL emission, and lower optical absorption. Flux zone technique is a halide free technique used for synthesizing truly semiconductor grade vdW crystals. This method distinguishes itself from chemical vapor transport (CVT) technique in the following regard: CVT is a quick (~2 weeks) growth method but exhibits poor crystalline quality and the defect concentration reaches to 1E11 to 1E12 cm-2 range. In contrast, flux method takes long (~3 months) growth time, but ensures slow crystallization for perfect atomic structuring, and impurity free crystal growth with defect concentration as low as 1E9 - 1E10 cm-2. During check out just state which type of growth process is preferred. Unless otherwise stated, 2Dsemiconductors ships Flux zone crystals as a default choice. 


XRD data collected from ZrSe2 crystals

zrse2-xrd.png

Raman spectrum collected from ZrSe2 layered crystals

zrse2-raman-spectrum.png

 
View AllClose

Additional Information

Elements:
Zr,Se
Element:
Zirconium
Element:
Selenium
Formula:
ZrSe2
Material class:
MX2
Material class:
Dichalcogen
Properties:
Semiconductor
Band gap range:
VIS
Growth method:
CVT
Growth method:
Flux
Doping:
Undoped
View AllClose